{Rearrangement of the antiferromagnetic ordering at high magnetic fields in SmFeAsO and SmFeAsO
0.9F
0.1 single crystals
Torque and magnetization measurements on SmFeAsO and superconducting SmFeAsO$_{0.9}$F$_{0.1}$ single crystals up to 60~T reveal a distinct rearrangement of the Sm antiferromagnetic ordering near 35–40~T. This field-independent transition appears as a sharp torque sign change and a magnetization jump, indicating a canted or partially polarized state. The saturation moment suggests full suppression of Sm antiferromagnetism requires fields above 60~T, remarkably large relative to the $T_{\rm N}\simeq5$~K, pointing to anisotropic exchange. Magnetoresistivity shows a sign crossover at the transition, evidencing coupling between Sm moments and FeAs-plane charge carriers.